IZBOR IZDELKOV
Izdelek |
Kem. osnova | Viskoznost pri 23°C (mPas) | MFFT (°C) | Zamreženje | Uporabnost mešanice | Odprti montažni čas (min) | Čas stiskanja
(min) |
Trajnostni razred po
EN 204 |
Posebne lastnosti |
MEKOL 1120 |
Disperzija PVAC | 7500–10.500 | Pribl. 8 | / | / | 7–10 | 15–20 | D2 | Visoka hitrost lepljenja |
MEKOL 1131 | Disperzija PVAC | 7000–10.000 | Pribl. 6 | Mekol B10 | Pribl. 8 ur | 7–10 | 15–30 | D3/D4 |
Watt’91 (80 °C) > 7 N/mm2 |
MEKOL 1133 |
Disperzija PVAC | 7000–10.000 | Pribl. 6 | Mekol B10 | Pribl. 8 ur | 10–12 | 15–30 | D3/D4 | Watt’91 (80 °C)
> 7 N/mm2 |
MEKOL 1141 | Disperzija PVAC | 10.000–14.000 | Pribl. 5 | Mekol B11 | 3–4 dni | 7–10 | 20–40 | D4 |
Watt’91 (80 °C) > 7 N/mm2 |
MEKOL 1144 |
Disperzija PVAC | Pribl. 7000 | Pribl. 6 | / | / | 10 – 12 | 20 – 40 | D4 | enokomponentno lepilo,
Watt’91 (80 °C) > 7 N/mm2 |
MEKOL 1163 | Disperzija PVAC | 7000–10.000 | Pribl. 5 | / | / | 7–10 | 15–30 | D2 |
Visoka trdnost spoja |
MEKOL 1152 |
Disperzija EPI | 5000 – 8000 | <0 | Mitopur B7 | 40 – 60 minut | 20 – 25 | 45 – 60 | D4+ | Visoka temperaturna odpornost spoja,
težje lepljive površine |
MITOPUR E45 | Prepolimer 1K PUR | 5500–9000 | / | / | / | 45–50 | 45–60 | D4+ |
Težje lepljive površine, ekstremni klimatski pogoji |